This document describes the method of determining the etch pit density, which is used to detect the dislocations and processing-introduced defects that occur on single-crystal GaN substrates or single-crystal GaN films. It is applicable to the defects specified in AWI 5618-1 from among the defects cropped out on the surface of the following types of GaN substrates or films: single-crystal GaN substrate; single-crystal GaN film formed by homoepitaxial growth on a single-crystal GaN substrate; or single-crystal GaN film formed by heteroepitaxial growth on a single-crystal Al2O3, SiC, or Si substrate. It is applicable to defects with an etch pit density of 7 × 107 cm-2 or lower.

Informations générales

  •  : Projet
    Vous pouvez contribuer à l’élaboration de ce projet de Norme internationale en contactant le membre national
    : Mise au vote du DIS: 12 semaines [40.20]
  •  : 1
     : 31
  • ISO/TC 206
    81.060.30 
  • RSS mises à jour

Prévisualiser 

Prévisualiser cette norme sur notre Plateforme de consultation en ligne (OBP)

Vous avez une question?

Consulter notre FAQ

Service à la clientèle
+41 22 749 08 88

Horaires d’ouverture:
De lundi à vendredi - 09:00-12:00, 14:00-17:00 (UTC+1)