Abstract
The temperatur above which the glass is capable of most forming operations is determined by measuring the elongation of a round glass fibre under its own weight. Closely defines requirements for the test specimen, procedure and apparatus lead to optimum repeatability of the specified temperature point. The furnace is specified with essential aspects.
General information
-
Status: PublishedPublication date: 1987-12Stage: International Standard confirmed [90.93]
-
Edition: 1Number of pages: 6
-
Technical Committee :ISO/TC 48/SC 7ICS :81.040.01